EFFECT OF SOME MACROMOLECULAR COMPOUNDS AND AMINO-ACIDS ON THE PITTING CORROSION OF ZINC IN CRO-4-2-/C1- MEDIUM

EFFECT OF SOME MACROMOLECULAR COMPOUNDS AND AMINOACIDS ON THE PITTING CORROSION OF ZINC IN CRO42/C1 MEDIUM

Authors

M E IBRAHIM

S MOHAMED

Published: June 01, 1986
Volume: 1986
Issue: 2 (JUN 1986)
Pages: 191
Region: e

Abstract

The anodic polarization technique was used to study the behaviour 2-2of Zn electrode in Cr04 and Cr04 /Cl solutions. The results revealed that in cro/- solutions two different types of behaviour were recorded. The addition of halides e.g. Cl-, Br-, r to cro/- sollltions was also studied. The aggressivness of the three halides were in the following order Cl > Br- > r-. A linear relation was obtained according to the following equation: E = a - b log C where: E the pitting potential, a and bare p agg. P constant. C is the concentration of the aggressive anion. The effect of agg starch, gelatine, poly (vinyl alcohol), glycine, L-alanine and L-valine was studied to elucidate which of these additives can inhibit or promote the corrosion process of Zn electrode in crO/-/Cl- solutions. The results revealed that glycine and L-alanine retarded the corrosion of zinc in crO/-/Cl- solution. This was indicated by the decrease of the critical current with increasing concentration while L-valine was found to be of no effect. On the other hand, two effects were obta i ned when macromo 1 ecu 1 ar compounds were used, whereas gelatine retards the corrosion, starch and poly (vinyl al~ohol) (P.V.OH) accelerate the process.

Keywords

EFFECT OF SOME MACROMOLECULAR COMPOUNDS AND AMINO-ACIDS ON THE PITTING CORROSION OF ZINC IN CRO-4-2-/C1- MEDIUM
Download PDF

How to cite this article:

M E IBRAHIM, S MOHAMED. (1986). EFFECT OF SOME MACROMOLECULAR COMPOUNDS AND AMINO-ACIDS ON THE PITTING CORROSION OF ZINC IN CRO-4-2-/C1- MEDIUM. JCSP Journal , 1986(2), 191 .

Related Articles

Role of Enzymatic System of Screened Pleurots ostreatus IBL-02 in the Bio-Removal of Synthetic Dyes Effluent

White rot fungi have exclusive capacity to decolorize synthetic azo dyes. Five different fungal strains namely S. commun...

Jun 01, 2019

Modeling of a Nickel-based Fluidized Bed Membrane Reactor for Steam Methane Reforming Process

Hydrogen being a green fuel is rapidly gaining importance in the energy sector. Steam methane reforming is one of the mo...

Apr 01, 2019

Ferrocene derivatives: Potential anticancer material

The presented work is focused on the investigation of ferrocene and its derivatives (ferrocene benzoic acid and ferrocen...

Dec 01, 2018

Application of Acid Dyes on Nylon Fabric and Evaluation of Fastness Properties Part III

A series of novel acid dyes, based on substituted aryl amines as diazo component and aminohydroxy-naphthalene sulfonic a...

Oct 01, 2018